Digital Library Publications
Automatic Detection Of Small Inclusions In Samples Of Optical Glass
F-T Lentes & H-J Becker
Special Glass
Redox Reactions Between Cations Of Different Polyvalent Elements In Glass Melts: An Optical Basicity Study
F G K Baucke
Special Glass
Surface Topography Of Polished And Oxide-Coated Bk-7 Glasses Investigated By Atomic Force Microscopy
O Anderson, K Bange
Special Glass
Characterization Of Thin Oxide Films On Glass: A Part Of The Problem-Solving Process
Dr K Bange
Special Glass