Digital Library Publications
How To Prevent Spontaneous Breakage Of Thermally Toughened Alkaline Earth Silicate Glass
U Gelderie & A Kasper
Special Glass
Chemical Behaviour Of Nickel Sulfide In Soda-Lime-Silica Glass Melts
A Kasper & H Stadelmann
Special Glass
Contribution To The Characterisation Of Dust Emissions Of Glass Melting Furnaces
A Kasper Et Al
General