Digital Library Publications
A Rapid Method For Accurate Determination Of Boron In Glass, Enamel And Other Silicate Materials
B Mitra, B C Sinha
Special Glass
A Gravimetric Method For Determination Of Water In Phosphate Glasses
D Kundu, S K Roy
Special Glass
Release Of Zinc And Phosphate Ions From Zno-P2O5 Glass Systems And Its Characterization
D Kundu, S K Roy
Special Glass
Properties Of Glasses And Melts In The System Mgo-Aln-Sio2
J Mukerji, Pk Das, D Chakraborty
Special Glass
Crystallization Of Glass In Fireclay Refractories: 1. Preliminary Observations On The "Synthetic" Glass
S P Chaudhari, T Datta
Refractories
An Analysis Of Short-Length Strength Distribution And Prediction Of Long-Strength Of Optical Fibres
K K Phani, A K De
Glass Fibre
Crystallisation Of Mgo-Al2O3-Sio2 Glass With Copper Oxide As Nucleating Agent
A K De
Glass Ceramics