A simple gravimetric method for determining water in phosphate systems has been developed.
Origin
Central Glass And Ceramic Research Institute, Calcutta
Journal Title
Trans Indian Ceram Soc 1988 47 5 147-148, 155
Sector
Special Glass
Class
S 270