Digital Library Publications
Adsorption Properties Of Chromatographic Sorbents Composed Of Thermally Treated Porous Glass And Chemically Bonded Carbowax 20M
A L Dawidowicz, I Choma, W M Buda
Special Glass
Surface Charge Studies On Lead Borosilicate Glass Containing Trace Sodium
M Shimbo Et Al
Special Glass
Influence Of Doping On The Interaction Betwen A Bioactive Glass And A Simulated Physiological Solution: Chemical And Epr Tests
J Krajewski Et Al
Special Glass
Some Properties Of Rf Planar Magnetron Sputtered Corning 7059 Glass Films
H Jerominek Et Al
Special Glass
Enhancement Of Lithium Conduction In Borate Glasses By Chloride: An Effect Of Network Dilation Or Bonding Strength Variation?
W Muller Et Al
Special Glass
Efficient Frequency Up-Conversion Via Energy Transfer In Fluoride Glasses
R S Quimby, M G Drexhage, M J Suscavage
Special Glass
Effects Of Copper And Lead On The Properties Of As-Ge-X Glasses (X=S,Se, Te)
B V Kobrin Et Al
Special Glass