Influence Of Doping On The Interaction Betwen A Bioactive Glass And A Simulated Physiological Solution: Chemical And Epr Tests

Chemical and EPR analyses indicated that the mineralisation phenomena around the bioglasses in the tissues also occur at an inorganic level.