Digital Library Publications
Corrosion Of Zinc-Containing Cabal Glasses By Various Leaching Solutions
A A Kheder Et Al
Special Glass
Dissolution Kinetics Of Some Industrial Glasses By Sodium Hydroxide Solution
H A Elbatal Et Al
Special Glass
Effect Of Thermal Neutrons On Vickers Microhardness Of Some Ternary Borate Glasses
H A Elbatal Et Al
Special Glass
Interaction Of Gamma Rays With Calcium Aluminoborate Glasses Containing Holmium Or Erbium
H A El-Batal Et Al
Special Glass
Interaction Between Lead Crystal Glass (24%Pb0) And Acetic Acid
A A Ahmed & I M Yossof
Domestic glass