Digital Library Publications
Rheological Properties And Isochomal Workability Of Lead Silicate Glass Melts
Y Yue & R Bruckner
Special Glass
Influence Of Homolgous Substitutions Of Chemical Components On The Rheological Properties And On Isochomal Workability Of Silicate Glass Melts
Y Yue & R Bruckner
Special Glass
On The Different Descriptions Of The Non-Newtonian Viscosity (Shear-Thinning Effect) Of Glass Melts With Respect To Heat Dissipation
Y Yue & R Bruckner
General
Which Rheological Parameters Control The Isochomal Workability Of Glass Melts From The Container Glass Industry?
Y Yue & R Bruckner
Container glass