Glass melts of various homolgous silicate glass series were investigated by means of the cylinder compression method with respect to their flow behaviour (Newtonian and non-Newtonian), stress generation modulus (stiffness, brittleness) and critical deformation rate (high-temperature tensile strength, isochomal workability).
Origin
Technische Universitat, Berlin
Journal Title
Glastech Ber Glass Sci Technol 69 7 1996 204-215
Sector
Special Glass
Class
S 1056