Digital Library Publications
An Analytical Study Contributing To The Understanding Of The Phenomenon Of Edge Corrosion Of Mirrors With Bevelled Edges (In Italian)
F Geotti-Bianchini
Special Glass
Experience In The Analysis Of Soda Lime Glass Surfaces In Connection With Industrial Problems
F Geotti-Bianchini
Special Glass
Parameters Affecting The Workability Of Container Glass. Part 2. Influence Of Dissolved Gases And Of Other Parameters.
F Geotti-Bianchini
Container glass
Parameters Affecting The Workability Of Container Glass. Part 1. Description Of The Problem - Melting History, Rheology And Influence Of Microstructure
F Geotti-Bianchini
Container glass