Digital Library Publications
British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.
Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:
- worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
- statistics – eg import/export data and recycling rates
- factory data – including types of glass manufactured, production capacities
- technical information on glass manufacture, material science, production techniques, compositions, decoration
- patents – including searches going back to the 19th century.
If there is something specific we can help with, email [email protected]
If you're not a member, we may still be able to help. Get in touch to find out more.
You can search our online database of articles, view abstracts, and order copies of articles using the search function below.
View our latest abstracts
Corrosion Of Molybdenum Electrodes In Glass Melts: Reaction Products And Effect Of Alkalies
J Matej Et Al
General
Corrosion Of Molybdenum Electrodes In Lead Glass Melts. Part 2. Effect Of Potential And Transfer Of Alternating Current By The Electrode
J Matej Et Al
General
Electrochemical Study On The Corrosionof Molybdenum Electrodes In Tv Glass Melts Containing Antimony
M Yamamoto Et Al
General