Digital Library Publications
Thermochemistry Of The Glass Melting Process - Energy Requirement In Melting Soda-Lime-Silica Glasses From Cullet-Containing Batches
C Madivate Et Al
General
Experimental Study On The Effect Of Cullet And Batch Water Content On The Melting Behaviour Of Flint And Amber Container Glass Batches
O Dubois & R Conradt
Container glass