It is shown that the principles of directed control of structure formation in materials by adding eutectic to modify their compositions are valid not only for aluminium oxide based ceramic, but also for ZrO2-based ceramic materials. The approaches considered for creating energy- and resource-efficient technologies serve as a reliable base for intensifying technological processes, lowering production costs, and increasing product quality.