A Fourier analysis of X-ray scattering by glasses in the system ZrF2-BaF2 is presented. Comparative discussions with crystalline structures of fluorozirconates are presented.
Origin
Unknown
Journal Title
Journal Of The American Ceramic Society 1983 66 (7) 523-529
Sector
Primary Papers
Class
PP 801