This firing method is designed to add soot to the natural gas flame to increase the flame emissivity, thus simultaneously increasing heat transfer, glass production rate, and thermal efficiency while lowering the peak flame temperatures and NOx emissions.
Origin
Combustion Tec Inc, Southern California Gas Co, Usa
Journal Title
Glass Industry 1992 74 3 31-33
Sector
General
Class
G 754