Weak Points Of Refractories In Glass Furnaces: Possible Ways Towards Solutions (Spanish)

The points of weakness of refractories installed in glass furnaces are outlined and possible approaches to overcoming the problems discussed. Corrosion phenomena are described with particular reference to surfaces exposed to attack by molten glass.

Author
D J C F Garcia
Origin
Cristaleria Espanola S.A.
Journal Title
Bol Soc Esp Ceram Vidr 1989 28 2 97-103
Sector
Refractories
Class
R 29