At the Societats-Druckerei printing centre in Frankfurn "Boresist" glass piping systems ensure that developing and fixing chemicals from the production of printing plates are removed without any problems.
Origin
Punktum Press Agency, Germany
Journal Title
Schott Information 77 1996 14-15
Sector
Special Glass
Class
S 1032