The unique properties of yttria-stabilized zirconia fibre and alumina-bonded alumina fibre products have extended their usefulness into applications too corrosive and demanding for other fibrous ceramic materials.
Origin
Zircar Prod Inc, Ny, Usa
Journal Title
Am Ceram Soc Bull 76 9 1997 79-82
Sector
Glass Fibre
Class
GF 177