This article looks at the AFM (Atomic Force Microscope - may also be referred to as SFM - Scanning Force Microscope) for studying glass surfaces.
Origin
Saint-Gobain Recherche
Journal Title
The Glass Researcher 9 1 1999 10, 20
Sector
Special Glass
Class
S 1779