New piezoceramic materials currently under development promise low intrinsic acoustic losses and high coupling factors that make them candidates for frequency control and selection applications in the burgeoning telecommunications market.
Origin
Us Army Communications, Nj
Journal Title
Am Ceram Soc Bull 83 9 2004 20-22
Sector
Glass Ceramics
Class
GC 601