The universal constants for metastable and stable phase separation have been derived from the lithium silicate, sodium silicate and barium silicate metastable systems and various stable systems in which the immiscibility boundaries have been measured.
Origin
Shanghai Institute Of Optics And Fine Mechanics
Journal Title
Phys Chem Glasses 1989 30 5 202-204
Sector
Special Glass
Class
S 316