Thermodynamic activity of the oxides of vanadium were studied in sodium borovanadate glasses equilibrated with V4+-V5+ redox system at 1000 and 1400 deg C in air.
Origin
Banaras Hindu University, India
Journal Title
Trans Indian Ceram Soc 59 4 (A) 2000 78-80
Sector
Special Glass
Class
S 2250