Since some basic properties of vitreous B2O3 depend very strongly on the stabilization temperature and the water content of the glass, one can exploit this fact to work with pure B2O3 as a model glass, studying how the glass-transition parameters and the physical properties of glasses vary with basic material parameter of the same substance.