The purpose of this article is to apply the polarisability approach developed by Dimitrov and Sakka to various tellurite (Te02) glasses.
Origin
Nagaoka University Of Technology, Japan
Journal Title
Phys Chem Glasses 42 2 2001 103-111
Sector
Special Glass
Class
S 2234