The thermal expanison behaviour of SiC fibre-reinforced Magnesium-Aluminium-Silicate (MAS) and Barium-Magnesium-Aluminium-Silicate (BMAS) glass ceramics was studied in air as well as in argon furnace atmosphere.
Origin
Inst Nichtmetallische Werkstoffe, Germany
Journal Title
Glastech Ber Glass Sci Technol 68 12 1995 404-409
Sector
Glass Ceramics
Class
GC 216