Physical and mechanical properties of glass-ceramics fabricated from thermal power plant fly ash were analysed and compared with a temperature-time-mechanical diagram.
Origin
Inha University, Korea
Journal Title
J Am Ceram Soc 88 5 2005 1227-1232
Sector
Glass Ceramics
Class
GC 621