Lithium magnesium metaborate glasses, xMg0.(1-x)Li20.B203 have been prepared by melt quenching in the 0
Origin
Nat Hellenic Research Foundation, Greece
Journal Title
Phys Chem Glasses 41 5 2000 321-324
Sector
Special Glass
Class
S 2068