A neutron inelastic scattering investigation of the superstructural unit concentrations in Cs2O-B2O3 glasses has been performed. Data have also been measured for crystalline caesium borates and used to identify the associated superstructural unit breathing modes in the neutron-weighted vibrational density of states (VDOS). Effective VDOS for vitreous caesium enneaborate and crystalline caesium pentaborate, measured at