Trials using different cleaning schedules have shown the advantage of introducing "dump rinsing" during the glass cleaning cycle in improving the quality of the components and seals and giving consistently higher yields.
Origin
Gec Avionics Ltd
Journal Title
Glass Technology 1990 31 2 44-48
Sector
Glass Ceramics
Class
GC 68