Study Of The Effect Of Heat Treatment And The Addition Of Iron On The Structure Of Vanadium Borophosphate Glass

Vanadium borophosphate glass samples with different iron oxide contents were prepared and heat treated at 350 degrees C for various times. X-ray diffraction and infrared spectroscopy were used to study the structure before and after heat treatment.

Author
A M Abo-El-Azm Et Al
Origin
Al-Azhar University
Journal Title
Phys Chem Glasses 1989 30 6 251-253