High resolution x-ray photoelectron spectroscopy has been used to investigate the structure of potassium and rubidium germanate glasses.
Origin
Lehigh University, Bethlehem, Usa
Journal Title
Phys Chem Glasses 37 5 1996 201-205
Sector
Special Glass
Class
S 1076