A neutron diffraction investigation of glasses in the Bi203-B203 system has been performed as a function of composition which confirms an earlier infrared study suggesting that BO4 tetrahedra are presented throughout the glass formation range.
Origin
Thomson Physical Labs, Reading, Uk
Journal Title
Phys Chem Glasses 41 6 2000 409-412
Sector
Special Glass
Class
S 2111