Glasses of high Na2O content in the sodium borate system have been prepared and studied by Raman and far infrared spectroscopy.
Origin
The National Hellenic Research Foundation
Journal Title
Phys Chem Glasses 1989 30 1 19-26
Sector
Special Glass
Class
S 216