Structural Models Of Selenite Glasses Containing Ag+ And Cu2 Ions

Selenite glasses are a new class of amorphous materials which are interesting mainly from a scientific point of view and they are not yet fully examined. Selenite glasses containing other non-traditional glass formers, as well as network modifiers were obtained. This study explains the glass formation ability in selenite systems with the participation of modifiers (Ag+ and Cu2+) and MoO3.

Author
A Bachvarova-Nedelcheva Et Al
Origin
Bulgarian Academy Sciences, Sofia
Journal Title
9Th Esg Conference, Trencin, Slovak Republic, June 2008 45-48
Sector
Special Glass
Class
S 3372

Request article (free for British Glass members)

Structural Models Of Selenite Glasses Containing Ag+ And Cu2 Ions
9Th Esg Conference, Trencin, Slovak Republic, June 2008 45-48
S 3372
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.