Stress Profile Characteristcs And Mechanical Behaviour Of Chemically Strengthened Lithium Magnesium Aluminosilicate Glasses

Chemically strengthened glasses were prepared by ion exchange in sodium nitrate and their stress profiles determined using the scattered light technique with a laser light source and surface removal by etching.

Author
M J C Hill, I W Donald
Origin
Atomic Weapons Establishment, Aldermaston
Journal Title
Glass Technology 1989 30 4 123-127
Sector
Special Glass
Class
S 299

Request article (free for British Glass members)