Crystallisation behaviour, especially spherulitic growth of a cordierite-3 mol% Y2O3-ZrO2 glass composition annealed at 950-1370 degrees C, was studied by optical and electron microscopy.
Origin
National Sun Yat-Sen University, Ind Technol Res Inst, Chufung
Journal Title
J Am Ceram Soc 1991 74 1 85-91
Sector
Glass Ceramics
Class
GC 87