Absorption and luminescence of chalcogenide glasses doped with neodymium were measured. Neodymium concentrations
Origin
Vavilov State Optical Inst, University Of Florida & Corning France
Journal Title
Corning Research 1997 65-71
Sector
Special Glass
Class
S 1430