The relationship of microstructure to service behaviour is discussed with reference to various silicate materials used in construction, including the weathering resistance of glass fibre reinforced concrete.
Origin
Purdue University
Journal Title
Proc Siliconf '90 9-21
Sector
Glass Fibre
Class
GF 55