Sodium Diffusion In The Nuclear Waste Glass Gp 98/12

The diffusion of 22Na was measured in the nuclear waste borosilicate glass GP 98/12 in the temperature range 350-450 degrees C.

Author
M P Thomas
Origin
Alcan International Ltd
Journal Title
J Am Ceram Soc 1989 72 1 146-147
Sector
Special Glass
Class
S 227