The local structure centred on sodium after diffusion in silica (Na-Si02 samples) has been determined by means of extended X-ray absorption fine structure (EXAFS) studies.
Origin
Lab Cnrs/Saint-Gobain, France
Journal Title
J Am Ceram Soc 85 5 2002 1041-1046
Sector
Special Glass
Class
S 2363