Different analytical techniques for the determination of sulphur balances of glass furnaces have been compared by the Technical Commission 13 (TC13 "Environment") of the International Commission on Glass (ICG). The calculation of sulphur balances are demonstrated for float glass and container glass furnaces. The results show the importance of accurate chemical analysis and mass flow measurements for cullet, glass, raw materials and filter dust to predict sulphur oxide emissions.
Origin
Tno Inst Appl Phys, The Netherlands
Journal Title
Glastech Ber Glass Sci Technol 72 10 1999 303-314
Sector
Special Glass
Class
S 1756