In the process of glass fibre forming the temperature distribution in bushing, tension of glass fibre and movement of glass strands are very important process parameters. Much cost has been involved in optimising these parameters. The purpose of this simulation model is to optimise these and improve the glass fibre forming process. This simulation model may also be utilised for saving costs and for developing better forming conditions.
Origin
Nippon Sheet Glass Co Ltd, Japan
Journal Title
Glass Tech 41 4 2000 135-139
Sector
Glass Fibre
Class
GF 246