Multicomponent (Ti, Zr, Al, B) silicon oxycarbide glasses and nanocomposite materials were derived after pyrolysis of gel hybrid structures in N2 atmosphere.
Origin
University Chem Tech & Metallurgy, Bulgaria
Journal Title
9Th Esg Conference, Trencin, Slovak Republic, June 2008 77-80
Sector
Special Glass
Class
S 3376