Different types of SiC whiskers are incorparated into lithium aluminosilicate and calcium aluminosilicate glass ceramics. The interfaces were characterised and the properties determined.
Origin
United Technologies Research Centre, Connecticut, Brown University
Journal Title
J Am Ceram Soc 75 5 1992 1205-1216
Sector
Glass Ceramics
Class
GC 119