Most glass producers all over the world use furnace insulation as a standard practice, trying to reduce the heat losses from the furnace walls to a minimum level. The glass furnace crown covers a large area of the furnace and when insulated significant savings of energy can be achieved.
Origin
Lubisol Engineering, Sofia, Bulgaria
Journal Title
Glass Sci Technol 76 6 2003 318-320
Sector
Refractories
Class
R 536