Rotational Faults In Hexagonal Bati03

Planar defects in the metastably retained h-BaTiO3 exhibiting a-fringe pattern have been characterized via transmission electron microscopy (TEM). The eligible fault vectors were determined by adopting the invisibility criteria augmented by high-resolution imaging. Three stacking faults, F1, F2 and F3, of the extrinsic nature have been fully analysed.

Author
Y Wu & H Lu
Origin
National Sun Yat-Sen University, Taiwan
Journal Title
J Am Ceram Soc 87 9 2004 1753-1763