Dynamic fatigue date are reported for fine- and coarse-grained micaceous glass-ceramics after contact damage with spheres.
Origin
Nist, Usa
Journal Title
J Am Ceram Soc 83 6 2000 1545-1547
Sector
Glass Ceramics
Class
GC 384