The Stratospheric Observatory for Infrared Astronomy (SOFIA) will be conducting a vast research programme during the next twenty years. On board is "Zerodur" mirror blank which fulfills all the conditions of the project.
Origin
Schott Glass, Mainz, Germany
Journal Title
Schott Information No 81 1997 6-7
Sector
Special Glass
Class
S 1257