The need to constantly improve the operating costs of glass furnaces and the application of ever stricter environmental regulations entail the use of reliable and efficient packing solutions in the regenerator chambers.
Origin
Sepr Glass Group
Journal Title
Glass Industry Development Int 2001 72-73, 75
Sector
Refractories
Class
R 385