With mounting environmental legislation, there is a growing need for advanced control over refractory production to achieve maximum efficiency. Controlling the particle size distribution of the refractory suspension is one key consideration and this article examines the use of a laser diffraction-based system for particle size analysis in the environment. The author explains how particle size analysis of refractory products could reduce costs and increase efficiency in manufacturing.
Origin
Malvern Instruments
Journal Title
Industrial Minerals Oct/09 74-75, 77
Sector
Refractories
Class
R 681